Why is the production of needle-punched non-woven fabrics uneven?

Home > News > Product knowledge  > Why is the production of needle-punched non-woven fabrics uneven?

Hot-sell product

Contact us

Guangzhou Junqian Nonwoven Co., Ltd.
Foshan Guide Textile Co., Ltd.

Sales Hotline: + 86-757-85700009
Customer Service Hotline: + 86-757-85756089
Email: sales2@guideco.cn
Address: Yonghao Industrial Park, Yongqing Rd., Yanbu, Dali Town, Nanhai Dist., Foshan, G.D. 528247, CHINA

Why is the production of needle-punched non-woven fabrics uneven?

2019-08-30 09:46:26
Needle-punched non-woven fabric(Non Woven Handicraft Felt Wholesale) is a kind of non-woven fabric. It is made of polyester and polypropylene raw materials and is processed by appropriate hot rolling after multiple times of acupuncture. Under the same processing conditions, why is the production of needle-punched nonwovens soft and hard? Let’s take a look!

Non Woven Handicraft Felt Wholesale, PP Needle Punch Non Woven Fabric Manufacturer, Diy Felt Fabric VendorNon Woven Handicraft Felt Wholesale, PP Needle Punch Non Woven Fabric Manufacturer, Diy Felt Fabric Vendor

Under the same processing conditions, the reasons for the unevenness of the production of needle-punched nonwoven fabrics(PP Needle Punch Non Woven Fabric Manufacturer) are as follows:

1. The low-melting fiber and the conventional fiber are unevenly mixed, the part with a higher low melting point content is harder, and the lower part is softer.

2. Incomplete melting of the low melting point fiber causes the needled nonwoven fabric(Diy Felt Fabric Vendor) to be soft.

3. The high shrinkage rate of the fiber also causes the problem of soft and hard unevenness of the needle-punched nonwoven fabric.

The above is the reason why the production of needle-punched non-woven fabrics will be uneven under the same processing conditions, I hope to help you.